Abstract:
A double-sided welding method for a solar cell sheet. The method comprises the following steps: arranging a bearing surface, which has a wire passing groove thereon, on an outer surface of a welding carrier; routing a first strip-shaped electrically-conductive connecting member in the wire passing groove; attaching the cell sheet to the bearing surface; tightly attaching a second strip-shaped electrically-conductive connecting member to an outer side surface of the cell sheet, and then compacting the cell sheet on the first strip-shaped electrically-conductive connecting member, which protrudes from the bearing surface, by means of the second strip-shaped electrically-conductive connecting member; and heating the first strip-shaped electrically-conductive connecting member and the second strip-shaped electrically-conductive connecting member, so as to weld the first strip-shaped electrically-conductive connecting member and the second strip-shaped electrically-conductive connecting member on the cell sheet.

Inventors:
WANG WEILIANG (CN)
CHEN ZHANGYANG (CN)
CAO YUHONG (CN)
Application Number:
PCT/CN2023/110135
Publication Date:
April 04, 2024
Filing Date:
July 31, 2023
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
CHANGZHOU SHICHUANG ENERGY CO LTD (CN)
International Classes:
B23K31/02; B23K37/04; H01L31/05; H01L31/18; B23K101/36
Foreign References:
CN115533360A2022-12-30
CN115483314A2022-12-16
DE102011081674A12013-02-28
CN85109495A1986-08-27
CN103038896A2013-04-10
CN215988800U2022-03-08
CN111531274A2020-08-14
DE202015106374U12015-11-27
Download PDF: